I am buring 110 mesh screens and trying to find the exposure time with my burning unit. I am coating with 1 pass on each side of the screen.

My burning unit is 4 - 48" flor. sunlight bulbs, placed 20" above the glass.

Does anyone have a similar set-up? or what would someone suggest as estimated burning time?


thanks!!!
User avatar
d fleming
Moderator
Moderator
Posts: 546
Joined: Mon Apr 03, 2006 3:33 pm

Post by d fleming »

Try a step wedge test starting at 11 minutes going to 18 & check results.